Hi all,
I will be going through a stage of refurbing some alloys soon. I plan on getting them shot blasted and then powder coated.
A few of the wheels have kurbing and also chunks taken from the face.
What is the best filler to use (when necessary) for shot blasting?
I don't want to make the wheels look perfect, and come shot blasting, have them destroy the filler!
When you pay professionals, what do they use to overcome such damage?
I will be going through a stage of refurbing some alloys soon. I plan on getting them shot blasted and then powder coated.
A few of the wheels have kurbing and also chunks taken from the face.
What is the best filler to use (when necessary) for shot blasting?
I don't want to make the wheels look perfect, and come shot blasting, have them destroy the filler!
When you pay professionals, what do they use to overcome such damage?